* TECHNICAL DATA
-------------------------------- 25 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 25
Yield / m2/kg(min.)/ - / : 62
Density / g/cm3 / ASTM D-1505 / : 0.6 -0.7
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 5.0
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,700
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 30 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 30
Yield / m2/kg(min.)/ - / : 51
Density / g/cm3 / ASTM D-1505 / : 0.6 -0.7
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 4.2
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,600
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 35 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 35
Yield / m2/kg(min.)/ - / : 44
Density / g/cm3 / ASTM D-1505 / : 0.6 -0.7
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 3.6
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,500
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 40 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 40
Yield / m2/kg(min.)/ - / : 38
Density / g/cm3 / ASTM D-1505 / : 0.6 -0.7
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 3.2
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,400
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
Description of Supply
Paper Core I.D. : 76 mm (3 in.) 152 mm (6 in.)
Roll O.D. : Max. 600 mm
Width Range : 100 mm - 1,500 mm.
(other width on request)
Length Range : Standard 4,000 m., 6,000 m.
Further technical information on request
Thank you and Best Regards,
Jim Kim
Sung Do International Co.,Ltd.
502-1, Mok-Dong, Yang Churn-Gu, Seoul, 158-807, Korea.
Tel : (82)(2) 2652-9482 / 9483
Fax : (82)(2) 2651-5648
e-mail : SDICOM@chollian.net
* BOPP CO-EX FILM PEARLIZED OPAQUE
Is widely used in surface printing for packaging application. Excellent machinability with both sides heatsealable. Our film show the pearlized white
opacity appearance.
* TECHNICAL DATA
-------------------------------- 25 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 25
Yield / m2/kg(min.)/ - / : 59
Density / g/cm3 / ASTM D-1505 / : 0.65 - 0.70
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 5.0
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,700
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 30 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 30
Yield / m2/kg(min.)/ - / : 49
Density / g/cm3 / ASTM D-1505 / : 0.65 - 0.70
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 4.2
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,600
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 35 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 35
Yield / m2/kg(min.)/ - / : 42
Density / g/cm3 / ASTM D-1505 / : 0.65 - 0.70
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 3.6
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,500
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
-------------------------------- 40 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 40
Yield / m2/kg(min.)/ - / : 37
Density / g/cm3 / ASTM D-1505 / : 0.65 - 0.70
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / ASTM D-1894 / : 0.40-0.60
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 26
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 3.2
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,400
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
Description of Supply
Paper Core I.D. : 76 mm (3 in.) 152 mm (6 in.)
Roll O.D. : Max. 600 mm
Width Range : 100 mm - 1,500 mm.
(other width on request)
Length Range : Standard 4,000 m., 6,000 m.
Further technical information on request
Thank you and Best Regards,
Jim Kim
Sung Do International Co.,Ltd.
502-1, Mok-Dong, Yang Churn-Gu, Seoul, 158-807, Korea.
Tel : (82)(2) 2652-9482 / 9483
Fax : (82)(2) 2651-5648
e-mail : SDICOM@chollian.net
* BOPP CO-EX FILM PEARLIZED OPAQUE HIGH GLOSS
Is widely used in surface printing and lamination for
medium speed packaging application. Excellent
machinability with one side heatsealable at low
temperature. Our film show the pearlized white opacity
appearance.
* PROVISIONAL TECHNICAL DATA
-------------------------------- 25 MICRON
Typical Properties/ Unit/ Test Methods/ Typical Value: /
Thickness / Micron / Micrometer/ : 25
Yield / m2/kg(min.)/ - / : 59
Density / g/cm3 / ASTM D-1505 / : 0.65 - 0.70
Tensile Strength / kg/mm2 / MD ASTM / : 6
/ (min.) / TD D-882-83 / : 12
Elongation at break / % / MD ASTM / : 140
/ (max.) / TD D-882-83 / : 50
Thermal Shrinkage / % / MD ASTM / : 4.0
/(120 ℃15 minutes)/ (max.) /TD D-1204-84 / : 2.0
Static C.O.F. /film/film / Treated / ASTM D-1894 / :
0.30-0.50
Static C.O.F. /film /film / Untreated /ASTN D-1894 / :
0.50-0.70
Sealing Temperature / ℃ / 1 Bar 1 Sec / : 115
Sealing Strength / g/cm(min.) / - / : 80
Gloss (Angle 45 ˚) / % (min.)/ASTM D-2457-70 / : 65
WVTR /g/m2/24 hr (max.) /ASTM E-96 / : 5.0
O2TR / cc/m2/24 hr (max.) /ASTM D-1434 / : 1,700
Corona Treatment /Dyne/cm (min.)/ ASTM D-2578 / : 38
Description of Supply
Paper Core I.D. : 76 mm (3 in.) 152 mm (6 in.)
Roll O.D. : Max. 600 mm
Width Range : 100 mm - 1,500 mm.
(other width on request)
Length Range : Standard 4,000 m., 6,000 m.
Further technical information on request
Thank you for your kind attention.
With Best Regards,
Jim Kim
Sung Do International Co.,Ltd.
502-1, Mok-Dong, Yang Churn-Gu, Seoul, 158-807, Korea.
Tel : (82)(2) 2652-9482 / 9483
Fax : (82)(2) 2651-5648
e-mail : SDICOM@chollian.net
Homepage : http://www.ec21.com/sdicom
|
 Related Keywords:
Surface Printing
,
Food
,
Packaging
,
Lamination
,
Meat
,
Chemicals
,
Coffee
,
Candies
,
Box
,
Sealing
,
Confectionery
|
|
|
| |
|
|
|